Hey everyone,
I’m Jake, and I run a small but scrappy HTCC packages supply operation—we work with everyone from startups cranking out next-gen wearables to automotive OEMs building the EVs of tomorrow, and honestly, one question I get way too often is: “How the hell do you even put together large HTCC packages without messing them up?” Large HTCC (High Temperature Co-fired Ceramic, for the new folks here) isn’t like slapping a few resistors on a PCB and calling it a day. These things are used for power modules, high-frequency comms, and aerospace parts—so if a single layer is off, you’re looking at a dead component, or worse, a product that fails mid-use.
Over the last 7 years, we’ve assembled thousands of large HTCC packages (think 50x50mm and up, not those tiny 10x10mm ones for phone antennas) and fixed a whole bunch of botched jobs from guys who skipped a key step or cut corners on materials. Today I’m breaking down the actual, no-BS process we use—stuff we learned the hard way, not just some textbook theory. No fancy jargon overload, just the real deal from a supplier who’s seen it all. HTCC Packages

First, let’s get one thing straight: large HTCC packages don’t work the same as their small cousins. Small ones are usually pick-and-plated in 2D with quick firing, but large formats? They warp. Like, a lot. We had a client once send us a batch they assembled in-house that came out 2mm off-square—they tried cramming it into a heat sink and it split down the middle. That’s the mistake everyone makes: treating large HTCC like a scaled-up small HTCC part. Big = different rules.

Step 1: Prepping the Green Tapes—This Is Where 80% of The Problems Start
Green tapes are the raw, unfired ceramic sheets you build the layers with. For large HTCC, you can’t just grab a standard roll and go. First, pick the right tape thickness. We use 0.2mm tape for anything over 40x40mm; thinner tapes flex too much when you’re punching vias, and thicker ones add unnecessary weight. Next, you have to degas the tape before punching. I know, sounds weird, but if there’s air trapped in the tape, when you punch vias (those tiny holes that connect layers), the tape tears, and you end up with little partial holes that will cause shorts later.
How we do it: We unroll the tape onto a flat vacuum table, leave it under suction for 2 hours at room temp. No heating—heat makes the tape stretch unevenly. Then, when we punch vias, we use a carbide die with a slight bevel on the edges. Sharp dies make clean holes, but large tapes need that bevel to stop the edges from chipping. Pro tip: Don’t punch all vias at once. For a 50x50mm package, punch half the vias, flip the tape, punch the other half. This avoids stretching the tape and warping it before you even get to layer registration.

Step 2: Layer Registration—Don’t Just Line Up Corners
This is the make-or-break step for large HTCC. Textbooks say “register layers to 10μm tolerance” but no one tells you how to actually do that without wasting 10 rolls of tape. When I started, we used a simple camera-aligned press, but we still had 1 in 10 layers misaligned. Then we got a laser registration system, and that changed everything. Here’s the trick: For large packages, you don’t just use the corner alignment marks. Use the mid-side marks too. A 50mm tape that’s 10μm off at the corner might be 25μm off at the middle edge, and that’s enough to throw off the entire stack.
We also use a 3-point clamping system instead of edge clamps. Edge clamps pull the tape unevenly, making it warp as you stack. 3 points (top-left, bottom-right, center) pull the tape flat without distorting it. And before you press layers together, always do a dry run: stack 2 layers, hold them up to the light. If light leaks through any spot, they’re off. Fix it before you press—once you apply pressure to 2 layers, you can’t adjust them without cracking the ceramic.

Step 3: Stacking and Laminating—Slow and Steady Beats Fast and Furious
Laminating large HTCC stacks is not a race. Most new assemblers want to crank up the pressure and heat to get it done in 10 minutes, but that’s how you get a warped stack. Large stacks have more material to squeeze, so uneven pressure will make some layers compress more than others.
We use a cold isostatic press (CIP) at our facility, but we do it in stages: First, a low-pressure cold lamination at 500 psi for 5 minutes just to hold the layers in place. Then, we move it to a vacuum hot press, heat it to 80°C, and apply 1000 psi for 15 minutes. No higher heat—hotter temps make the binder in the tape evaporate too fast, leaving bubbles in the stack. After lamination, we let the stack cool slowly for 8 hours, not 1 hour. Rapid cooling causes thermal stress, which leads to cracks during firing. I learned this the hard way: our first large batch came out of the press, we slammed it on a table to speed up cooling, and 3 out of 12 stacks had hidden cracks that showed up during testing. Never again.

Step 4: Binder Burnout—The Hidden Cause of Firing Failures
Binder burnout is when you heat the stack to burn off the organic binder in the green tape. For small HTCC, you can do this in 2 hours, but large stacks need 12+ hours. Why? The binder has to escape through the surface of the stack, and a thick stack can’t let it out fast. If you heat too fast, the binder boils inside the stack and blisters the ceramic.
We have a custom burnout oven for large formats. The first 6 hours, we hold the temp at 300°C—slowly letting the binder evaporate. The next 4 hours, we ramp up to 600°C to burn off the remaining binder. For the last 2 hours, we hold at 600°C to make sure nothing’s left. We test the off-gas too—if the CO2 level drops to zero, we know the binder is gone. Skip that test, and you’ll have leftover carbon that turns your ceramic gray and causes conductivity issues later.

Step 5: Firing—Avoiding Warp Like Your Job Depends On It (It Does)
This is where most large HTCC jobs go wrong. Firing shrinks the ceramic, and large packages shrink unevenly if the oven is not set up right. Textbooks say “uniform temp throughout the oven,” but we’ve found that for large stacks, you need to offset the temp by 5°C at the bottom and top of the oven to compensate for heat stratification.
Our firing cycle is: ramp from room temp to 1550°C over 10 hours, hold at 1550°C for 2 hours, then cool for 12 hours. No fast ramps. For large packages, we also place a setter plate under the stack. Setter plates are made of the same ceramic as the HTCC, so they shrink at the same rate. If you use a different material, it will shrink differently and warp your package. We’ve tried using alumina setters before—big mistake. The alumina shrank 2% more than our HTCC, and we ended up with 10mm warps on 50mm packages. Never again, stick to matching setter material.

Step 6: Post-Firing Processing—Cleaning and Testing That No One Talks About
Once the packages are fired, you can’t just take them out and start attaching parts. First, you have to de-flash. Flash is the tiny ceramic residue left on the edges after firing. For large packages, we use a sandblaster with 50μm alumina grit—too big and it scratches the surface, too small and it doesn’t remove the flash. We also do a laser trim to adjust the edge dimensions to ±5μm tolerance. That’s important for mating with heat sinks or housings.
Then testing is non-negotiable. We do 3 tests: first, a visual inspection under a 50x microscope to look for cracks or missing vias. Second, a continuity test for all vias—even one bad via ruins the package. Third, a warpage test with a coordinate measuring machine (CMM). We accept a maximum warp of 0.1mm per 50mm package—anything over that is scrapped. We had a client once ask us to ship packages with 0.2mm warp, saying they’d sand the edges to fit. We refused—those packages would crack when soldered, and they’d blame us. It’s better to be picky.

A Quick Note On Common Mistakes We See All The Time
Let’s wrap this up with the stuff that makes us want to facepalm when we get inquiry emails:

  1. Scaling up small HTCC processes: Large is different—you can’t just use a bigger pick-and-place or press.
  2. Cutting corners on prepping green tape: Degassing is not optional, it stops tears.
  3. Skipping the binder burnout test: Leftover carbon = bad components.
  4. Using mismatched setter plates: They cause warps, period.

If you’re looking for reliable large HTCC packages—ones that go through every step we talked about, no cutting corners—hit us up. We work with startups, aerospace teams, automotive guys, whoever needs consistent, high-quality HTCC for their projects. No run is too big or too small, and we’re happy to walk you through the process if you’re new to working with large format ceramic.

Leadless Ceramic Packages References

  1. High Temperature Co-fired Ceramic (HTCC) Technology and Applications, Ceramic Industry Association
  2. Process Guidelines for Large Format Ceramic Packaging, International Microelectronics and Packaging Society
  3. Warpage Mitigation in Thick Ceramic Substrates, Journal of Microelectronics and Electronic Packaging

Tessvida Technologies Pte. Ltd.
As one of the most professional htcc packages manufacturers and suppliers, we also support custom service and OEM service. Please feel free to buy high quality htcc packages at competitive price from our factory. Welcome to view our website for more information.
Address: 5008, Ang Mo Kio Ave.5, #04-09, Techplace II, Singapore 569874
E-mail: info@tessvida.com